BATA鸿贝蓄电池缺液阴碍情形及排除方法:


  鸿贝蓄电池是经过铅与二侵蚀铅进行通化硫化而放电的设备。蓄电池酸液也即是电解液的比重(酸液和蒸馏水畸形的比例是0.125)。由于温度高会导致电解液中的水份蒸发,这时就会紧要增多蒸馏水,这属于正常现象。要是是某些操纵招致了电解液成分消散概略电解液因素浓度更改,这时候就泛起了缺液故障。

鸿贝蓄电池亏电症状:

1、 敲击电池有浮泛响声

2、 电池份量显著加剧

排查原因:

1)电池外壳损伤开裂(更换安装电池碰伤或底部有凶猛物)

2)电池永劫日歪斜逾越45度,导致电解液从排气孔流出

3)鸿贝电池容量与负载不适配,导致电池组出现“小马拉大车”

4)电池过充电(现实输出电压大于14.4V)

 Battery failure can be divided into three reasons: the first is quality problems, such as leakage and micro-short circuit.Generally speaking, the grounding system of UPS shall comply with the IEC60346 standard on low-voltage grounding system.This means that for most UPS, the center line of the battery pack and the battery rack are grounded.Therefore, when there is a battery leakage in the battery pack, and the leaked electrolyte flows to the battery rack, a short circuit will be formed between the battery pack to cause an accident.If there is a micro-short-circuit battery in the battery pack, the voltage of the micro-short-circuit battery will drop rapidly when the battery is discharged, resulting in insufficient standby time.

技术支持: 全国免费服务电话400-869-7656 | 管理登录
seo seo